Q.The method used for the concentration of sulphide ores is

(a) Hydraulic washing
(b) Leaching
(c) Magnetic separation
(d) Froth flotation
Kerala DhseKerala DHSE Plus Two Board 2022MCQ· 1mImportance★★★★★
0% · 0/35 Questions
🔒 Locked · start free trial →

You're viewing a preview — the full solution, concept, methods & PYQ mapping are locked.

Start your 14-day free trial to unlock the full solution →

Sulphide ores are concentrated by the froth flotation method, which exploits the preferential wetting of sulphide particles by oil/pine oil (and by frothing agents) over water.

In froth flotation, the finely powdered sulphide ore is mixed with water and a small amount of pine oil/collector (e.g. xanthates), then agitated with air. The sulphide ore particles are preferentially wetted by the oil and stick to the air bubbles, rising to the surface as a stable froth that is skimmed off. The gangue (impurity, e.g. silica), being preferentially wetted by water, settles at the bottom.

…

Unlock everything free for 14 days

  • Full step-by-step solutions
  • Concept-first explanations
  • Methods, shortcuts & mistakes
  • PYQ mapping + timed mock tests

Full access for 14 days. No credit card required.